KOMPOSISYONG KEMIKAL
incoloy 625 coiled tubing capillary tubing
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0.1 | 20 – 23 | ≥ 58 | ≤ 5 | ≤ 0.5 | ≤ 0.5 | 8 – 10 | ≤ 1* | ≤ 0.015 | ≤ 0.015 | ≤ 0.4 | 3.15 – 4.15 | ≤ 0.4 |
(mass%)
*Kung matukoy
Bawat ASTM B444, ASME SB444, AMS 5581
Kundisyon | Lakas ng makunat | Lakas ng Yield | Pagpahaba |
minimum, ksi | minimum, ksi | minimum, % | |
Baitang 1 | 120 | 60 | 30 |
Baitang 2 | 100 | 40 | 30 |
*Maaaring magbigay ng mas mataas na lakas ng mga katangian sa malamig na hardened na kondisyon.
70°F | 200°F | 400°F | 600°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Densidad | lbs/in3 | 0.305 | - | - | - | - | - |
Thermal Expansion | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Elastic Modulus | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Poisson Ratio | - | 0.278 | 0.28 | 0.286 | 0.29 | 0.295 | - |
Thermal Conductivity | Btu-in/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Tukoy na init | Btu/lb·°F | 0.098 | 0.102 | 0.109 | 0.115 | 0.122 | 0.118 |
Lakas ng Yield | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Lakas ng makunat | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 coiled tubing capillary tubing
PROSESODESCRIPTIONSteel MakingElectric Arc Furnace na sinusundan ng Vacuum Oxygen Decarburization (VOD) o Argon Oxygen Decarburization (AOD).Pipe MakingConventional Seamless Cold Finished Pipe and Tube Manufacturing Processes.Heat TreatmentHindi maaaring tumigas ng heat treatment.Maaaring ibigay sa annealed, solution annealed o cold hardened condition.Ang mas mataas na lakas ng annealed condition ay karaniwang ginagamit sa mga serbisyo hanggang sa 1100°F, habang ang solution annealed condition ay ginagamit sa mga application sa itaas ng 1100°F.